A single (Ba0.85Ca0.15)(Zr0.10Ti0.90)O3 phase material with a tetragonal structure is processed and synthesized with a modified Pechini method using ethylenediaminetetraacetic acid and glycerol as chelating and esterifying agents, respectively. The complete chemical transformation to the desired phase is achieved at 900 °C, which is 300 °C lower than conventional synthesis methods. Its consolidation, reaching up to 91% relative density, is carried out at 1400 °C. It is clearly demonstrated that the use of ethylenediaminetetraacetic acid and glycerol reagents is particularly beneficial for inducing a homogeneous grain size distribution (10 μm), which leads to very promising electromechanical properties (d33 = 451 pC/N; d31 = 160 pC/N; kp = 0.40; (Formula presented.) = 4790 and Qm = 358) of the densified system.

High Purity, Crystallinity and Electromechanical Sensitivity of Lead-Free (Ba0.85Ca0.15)(Zr0.10Ti0.90)O3 Synthesized Using an EDTA/glycerol Modified Pechini Method / Caggiu, Laura; Cau, Costantino; Mureddu, Marzia; Enzo, Stefano; Murgia, Fabrizio; Pardo, Lorena; Lopez-Esteban, Sonia; Bartolomé, Jose F.; Mulas, Gabriele; Orrù, Roberto; Garroni, Sebastiano. - In: MATERIALS. - ISSN 1996-1944. - 18:5(2025). [10.3390/ma18051180]

High Purity, Crystallinity and Electromechanical Sensitivity of Lead-Free (Ba0.85Ca0.15)(Zr0.10Ti0.90)O3 Synthesized Using an EDTA/glycerol Modified Pechini Method

Caggiu, Laura;Cau, Costantino;Mureddu, Marzia;Enzo, Stefano;Murgia, Fabrizio;Pardo, Lorena;Mulas, Gabriele;Garroni, Sebastiano
2025-01-01

Abstract

A single (Ba0.85Ca0.15)(Zr0.10Ti0.90)O3 phase material with a tetragonal structure is processed and synthesized with a modified Pechini method using ethylenediaminetetraacetic acid and glycerol as chelating and esterifying agents, respectively. The complete chemical transformation to the desired phase is achieved at 900 °C, which is 300 °C lower than conventional synthesis methods. Its consolidation, reaching up to 91% relative density, is carried out at 1400 °C. It is clearly demonstrated that the use of ethylenediaminetetraacetic acid and glycerol reagents is particularly beneficial for inducing a homogeneous grain size distribution (10 μm), which leads to very promising electromechanical properties (d33 = 451 pC/N; d31 = 160 pC/N; kp = 0.40; (Formula presented.) = 4790 and Qm = 358) of the densified system.
2025
High Purity, Crystallinity and Electromechanical Sensitivity of Lead-Free (Ba0.85Ca0.15)(Zr0.10Ti0.90)O3 Synthesized Using an EDTA/glycerol Modified Pechini Method / Caggiu, Laura; Cau, Costantino; Mureddu, Marzia; Enzo, Stefano; Murgia, Fabrizio; Pardo, Lorena; Lopez-Esteban, Sonia; Bartolomé, Jose F.; Mulas, Gabriele; Orrù, Roberto; Garroni, Sebastiano. - In: MATERIALS. - ISSN 1996-1944. - 18:5(2025). [10.3390/ma18051180]
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11388/360829
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 0
  • ???jsp.display-item.citation.isi??? 0
social impact